The edge crush test (ECT) measures how much load a strip of corrugated board carries on its edge before it buckles, and it is the best single guide to how well a box will stack. Burst strength measures resistance to rupture under pressure, which relates to puncture and rough handling. A sound specification states both.
Two figures on the same quote
Two quotes arrive for what looks like the same double wall carton. One states a burst strength in kPa, the other an edge crush value in kN/m, and a third supplier simply lists the paper make-up, a code such as 150K/150T. None of them is wrong, but they are not describing the same thing, and only one of them tells you directly whether the box will hold up under a stack.
The paper make-up describes the ingredients: the weight and type of each liner, kraft or test, and the fluting. It helps check that two quotes are built alike, but it does not state performance. Boards with similar codes can test differently, and a lighter code can outperform a heavier one. Performance is what the burst and edge crush figures are for, and made-to-size cartons through bespoke carton manufacture should carry both.
What is the edge crush test?
The edge crush test takes a small rectangular sample of corrugated board, cut so that the flutes run vertically, stands it on its edge between the plates of a compression tester and squeezes it until it buckles. The result is the maximum force the board carried per unit length of the loaded edge.
In the UK and Europe the standard method is ISO 3037, and results are given in kilonewtons per metre (kN/m). In the United States the equivalent test reports in pounds per inch (lb/in), and US box certificates often carry an ECT rating such as 32 or 44. One lb/in is about 0.175 kN/m, so ECT 32 is roughly 5.6 kN/m. Converting before comparing avoids a US datasheet being read as many times stronger than a UK one.
What drives an edge crush test rating
ECT depends mainly on the compression strength of the papers, the liners and the fluting medium together, which is measured on the paper itself by the short-span compression test (ISO 9895). The number of fluted layers matters too, which is why double and triple wall boards score far higher than single wall. Manufacturing quality plays a part: poorly bonded or crushed flutes lose edgewise strength before the box is ever filled.
ECT is a property of the board, not the box: how strong the material is in the direction a stacked wall is loaded, and the main input to estimating what the finished box will carry.
What burst strength measures
Burst strength, often called the Mullen test after the original instrument, clamps a piece of board over a rubber diaphragm and raises the pressure beneath it until the board ruptures. For corrugated board the method is ISO 2759, and the result is given in kilopascals (kPa). Older US specifications express it in pounds per square inch, so a "200 lb test" board is one rated at a 200 psi burst, about 1,380 kPa.
Burst is driven mostly by the tensile strength and weight of the liners. Heavier liners, and kraft rather than test liners, generally raise it. It is a good indicator of how the board copes with puncture, contents pressing outward and rough parcel-network handling. It does not measure resistance to load from above, because the force acts across the face of the board, not along its edge.
Edge crush test vs burst strength: which predicts stacking
A box in a stack fails when its side walls buckle under the weight above. That is edgewise compression, which is exactly what the edge crush test reproduces. Burst does not load the board that way at all, so two boards can share a burst value and differ widely in ECT. Heavy kraft liners on a light fluting can give a high burst with only a modest ECT, while a well-made board on lighter papers can stack better than its burst figure suggests.
| Consideration | Edge crush test (ECT) | Burst strength |
|---|---|---|
| What it measures | Load on the edge of the board before buckling | Pressure on the face of the board before rupture |
| UK and EU method | ISO 3037 | ISO 2759 |
| Usual UK / EU unit | kN/m | kPa |
| Usual US unit | lb/in (e.g. "ECT 32") | psi (e.g. "200 lb test") |
| Driven mainly by | Compression strength of liners and fluting, number of walls | Tensile strength and weight of the liners |
| Best predictor of | Stacking and box compression strength | Puncture, bulging contents, rough handling |
| Does not tell you | Puncture resistance | How the box holds up under a stack |
How ECT becomes box compression strength
The widely used estimate is the McKee formula, which relates box compression strength (BCT) to three things: the ECT of the board, the board's thickness (caliper) and the perimeter of the box. In principle, BCT rises in direct proportion to ECT and roughly with the square root of caliper multiplied by perimeter. Doubling the ECT roughly doubles the estimated box strength; thicker board helps, but less than proportionally.
The estimate assumes a well-made regular slotted case compressed evenly under laboratory conditions. Real stacks are less kind. Humidity, weeks under constant load, cartons overhanging the pallet edge, misaligned columns, handholes and large print areas all reduce the load a box will actually carry. A complete package can be compression tested under ISO 12048, but the number that matters is what the box holds after those losses, which is why a specification needs a margin and a description of the conditions.
Burst tells you whether the board will be punctured; edge crush tells you whether the box will hold up the ones above it.
Using both figures on a specification
Neither figure replaces the other. The practical approach is to decide which failure you are guarding against and set the relevant figure as a minimum, then record both so that reorders stay the same.
- Start from the stack. Work out the weight sitting on the bottom box, how long it stays there and in what conditions. That sets the box strength you need, and from it the minimum ECT.
- Add burst where puncture is the risk. Dense contents, parcel-network despatch and forklift handling are where a burst minimum earns its place.
- Name the standards. Ask for ECT to ISO 3037 and burst to ISO 2759, tested on board conditioned to the ISO 187 standard atmosphere of 23 °C and 50% relative humidity, so figures from different suppliers are comparable. Your own warehouse will rarely be that dry.
- Compare like with like. Convert lb/in and psi before comparing a US datasheet with a UK quote, and check flute and wall construction alongside the numbers.
- Put it in writing. A specification held on file is reordered as the same board, not decided again each time.
Reading a quote that only gives one figure
A quote that lists only burst is common, because it is the older and more familiar measure. If your cartons are palletised and stacked, ask for the ECT as well; it is the number that answers your actual question. A quote that lists only the paper make-up should be asked for both. If the figures you are offered look generous for the job, that is worth raising too: board specified above the load is cost on every box, and a packaging review often finds grades chosen by habit rather than by the stack.
For dimensions, flute and style, see how to specify a cardboard box; if cartons are already failing, start with stopping packaging being crushed in transit. Flute profiles are set out under packaging materials and the board range under corrugated packaging. The heaviest loads are specified on the same two figures under industrial packaging.
Have your box specification checked
Send us the quote or specification you have, the product weight and how the cartons are stacked. We will specify the board against the load and put the edge crush and burst figures in writing.
Frequently asked questions
What is the edge crush test?
A laboratory test that compresses a small strip of corrugated board on its edge, with the flutes vertical, until it buckles. The result, in kN/m under ISO 3037, shows how much load the board carries edgewise and is the best single guide to stacking strength.
What is the difference between edge crush test and burst strength?
Edge crush measures load along the edge of the board, which is how a stacked box wall is loaded. Burst measures the pressure needed to rupture the board face, which relates to puncture and rough handling.
What does an edge crush test rating of 32 mean?
It is a US rating in pounds per inch, so 32 lb/in, which is roughly 5.6 kN/m. UK and European specifications normally state edge crush in kN/m, so convert a US figure before comparing it with a UK quote.
Is a higher burst strength always better?
No. Higher burst usually means heavier or stronger liners, which helps against puncture but adds cost and does not guarantee stacking strength. If boxes are crushing in a stack, edge crush is the figure to raise.
Can I work out box compression strength from the edge crush test?
Approximately. The McKee formula estimates box compression strength from edge crush, board thickness and box perimeter. It is a starting point: humidity, time under load, pallet overhang and handholes all reduce real stacking strength.
Which test standards should a UK box specification quote?
ISO 3037 for edge crush and ISO 2759 for burst, on board conditioned to the ISO 187 standard atmosphere, so that figures from different suppliers can be compared directly.